shortage across insulation layers
2010-01-09
Dong Cai
2010-01-10
Prasanna Srinivasan
2010-01-09
Karolina psychowlosy
shortage across insulation layers
Prasanna Srinivasan
2010-01-10
Dong,

THis could have been due to dielectric break down. It depends on the voltage
you applied across the electrodes and the band gap of the dielectric
materials (alumina and SOG). How thick the layers are and how much voltage
you applied?

- Prasanna

On Sat, Jan 9, 2010 at 4:29 AM, Dong Cai  wrote:

> Hi,
>
> I have a 3D nanostructure made of carbon materials. Two dielectric layers
> are deposited on it. The first layer is 100 nm alumina by ALD, then the
> second one is spin-on-glass (512B). The chip was top covered by 200 nm
> silver film.  But I frequently measured a short between the top Ag and
> bottom carbon.
>
> Need help! Thanks!
>
> Dong

--
Thanks & Regards,
Prasanna Srinivasan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review