what CMOS compatible means exactly
2010-05-12
Yu Chen
2010-05-12
Alex Mellnik
2010-05-13
Robert Black
2010-05-14
Yu Chen
2010-05-14
Andrew Irvine
2010-05-14
Marc Reinig
2010-05-17
Rabah Hanfoug
what CMOS compatible means exactly
Rabah Hanfoug
2010-05-17
Dear Yu Chen,

In my opinion, from technology point of view, every CMOS technology has its own
design rules, modules and process procedure.

Compatible then means that you have to respect all those rules and process
procedures.

Regards
Rabah

> Date: Wed, 12 May 2010 13:55:05 +0800
> From: [email protected]
> To: [email protected]
> Subject: [mems-talk] what CMOS compatible means exactly
>
> I am wondering what CMOS compatible means exactly.
>
> Probably it includes:
>
> Materials: some materials are not allowed
>
> Process: some processes are not preferred like liftoff
>
> Temperature:
>
> …
>
> Any comments are welcome.
>
> Thanks
>
> Yu CHEN
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group