MEMSnet Home: MEMS-Talk: Damaged wafers after SC1 clean
Damaged wafers after SC1 clean
2010-10-21
Fradkin Evgenia - Golda
2010-10-21
Felix Lu
2010-10-21
Goodman, Lawerence
Damaged wafers after SC1 clean
Goodman, Lawerence
2010-10-21
If the peroxide concentration in the SC-1 drops too low, then it is known that
the silicon surface can be etched by the ammonia. Polycrystalline and amorphous
silicon are much more sensitive to this phenomenon.

L.Goodman
Sarnoff Corp.

-----Original Message-----
From: Fradkin Evgenia - Golda [mailto:[email protected]]
Sent: Thursday, October 21, 2010 3:04 AM
To: '[email protected]'
Subject: [mems-talk] Damaged wafers after SC1 clean

Hello,

We've encountered a serious damage to the wafers surfaces during SC1 cleaning
process.  A picture of a damaged silicon wafer after the cleaning process is
attached.
This damage occurs only for wafers from a certain vendor.

It seems that wafers from other vendors are damaged as well if being cleaned in
the same solution after the said damaged wafers.

Have anyone encountered such a problem before? Can you suggest what might be the
cause?

Thanks,

Evgenia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group