Cr/Au evaporation on diamond
Shay
2011-01-05
Andrea,

Either Cr or Ti should work

Shay

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Andrea
Mazzolari
Sent: Wednesday, January 05, 2011 7:39 PM
To: [email protected]
Subject: [mems-talk] Cr/Au evaporation on diamond

Hi all,

i would need to evaporate 80nm of Au on a thin diamond layer.
Cr is tipically used as adhesion layer while evaporating Au on Silicon.

Is a Cr adhesion layer needed also to evaporate Au on diamond ?
In the case Cr will not adhere on diamond, which other adhesion layer should
be used ?

Best regards,
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review