A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Image Reversal resist
Image Reversal resist
2011-02-23
Xiaohui Lin
2011-02-23
Bill Moffat
2011-02-23
Wilson, Thomas
2011-02-24
Warren Dustin
2011-02-24
[email protected]
2011-02-24
Bill Moffat
Image Reversal resist
[email protected]
2011-02-24
Maybe you can choose SU-8 2005?

I think that if you choose any negative resist, you can perform negative angle.


------Original Message------
From: Xiaohui Lin 
To: General MEMS discussion 
ReplyTo: Xiaohui Lin 
[mems-talk] Image Reversal resist
Feb 23, 2011 15:51

We are currently looking for a kind of resist that can form 6-8um THICK
NEGATIVE angle on substrate.

AZ9260 is able to provide thick resist but the developed shape is of
positive angle.

AZ5214 if using image reversal, is able to provide negative angle but its
thickness is always less than 2um.

I am just wondering if AZ9260 able to process with image reversal process?

Any other choice?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review