MEMSnet Home: MEMS-Talk: Finding [110] direction on (100) SOI wafer
Finding [110] direction on (100) SOI wafer
2011-03-14
Qi Luo
2011-03-15
Andrea Mazzolari
2011-03-15
Steckenborn, Arno
Finding [110] direction on (100) SOI wafer
Steckenborn, Arno
2011-03-15
Hi,

Look at this:

Mattias Vangbo and Ylva Bäcklund 1996 J. Micromech. Microeng. 6 279

Arno


An: General MEMS discussion
Betreff: [mems-talk] Finding [110] direction on (100) SOI wafer

Greetings everyone,

I would like to find out the exact [110] crystal direction of a (100) SOI wafer
before my first mask. The top Si (100) is about 200um thick. Wafer will come
with flat supposedly aligned to [110] direction, yet may have anyway from 0 to 3
degree alignment variation to [110]. Your suggestions would be greatly
appreciated.

Best regards,

--- Qi Luo

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group