deposition of SiO2 on n-GaN
2011-03-25
Jack
deposition of SiO2 on n-GaN
Jack
2011-03-25
Dear all,

   I have deposited a SiO2 passive layer on n-GaN without annealing (RTA
facility did not work). But that the passive layer is fragile for
postprocessing. I want to fabricate mental line on this layer, but when
lifting off the photoresist in developer, some cracks showed up. It seems
that the deposited thickness is the key issue which affects the quality of
SiO2.

   Anybody familiar with this field please give some suggestions.

--
Sincerely
Jack, Zetao MA
Dept.of EEE, CYC712,HKU
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer