Nickel electroplating on ITO glass
Bill Moffat
2011-05-05
When LCD adhesion to ITO became a problem the cure was to abrade the ITO
with a velvet glove.  I kid you not.  Then a move to a wet chemical
adhesion promoter OCTES.  Then a move to vapor OCTES for better
adhesion.  If the OCTES which is only one molecule thick  would not
impede the plating process, I can offer you a free trial of vapor OCTES.

Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of Xiaohui Lin
Sent: Wednesday, May 04, 2011 12:21 PM
To: General MEMS discussion
Subject: [mems-talk] Nickel electroplating on ITO glass

We need Nickle to be plated on a transparent substrate. Seems plating on
ITO renders bad adhesion.

Does anyone have any idea about the possibility of electroplating Ni on
ITO glass?  Specifically, how to improve the adhesion?

Thanks
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group