Hi all -

I'm trying to get photoresist (currently Shipley 5740, but any AZ type resist
would also be fine) to stick to a hydrophobic polymer (silicone).
Has anyone succeeded in doing this already?  Anyone have any suggestions of
what might be good to try?

Thanks in advance,

Marc Unger
[email protected]
Applied Physics
Caltech


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.