A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: make the su-8 surface flat
make the su-8 surface flat
2011-06-10
첸로
2011-06-10
Khaled Mohamed Ramadan
2011-06-10
Xiaohui Lin
2011-06-10
첸로
2011-06-10
Eric Johnston
2011-06-11
첸로
2011-06-11
dai truong
2011-06-12
gau s
2011-06-13
Shane GUO
2011-06-14
Khaled Mohamed Ramadan
2011-06-14
Shane GUO
2011-06-15
Gareth Jenkins
2011-06-15
Shane GUO
2011-06-16
첸로
2011-07-06
Le Hong Hanh
2011-07-12
Shane GUO
2011-07-16
Bill Moffat
make the su-8 surface flat
첸로
2011-06-11
Hello Eric,

what is the purpose of resting for one day? It will prevent the bead edge
diffuse into the inner?

Could you mind telling me in datail?

Thanks in advance
Kind Regards




At 2011-06-11 03:28:06,"Eric Johnston"  wrote:

>Hi.
>
>We spin coat then let the wafer rest for a day in a covered petri dish.
>Then soft bake.
>
>Eric
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group