MEMSnet Home: MEMS-Talk: ultra thin silicon membranes
ultra thin silicon membranes
2011-10-07
Andrea Mazzolari
2011-10-08
Marc Reinig
2011-10-08
Andrea Mazzolari
ultra thin silicon membranes
Andrea Mazzolari
2011-10-08
Hi Marc,

that is exactly the paper i cited in my first e-mail to memsnet group ;)

I wish to find other papers and potential applications.

Best regards,
Andrea

> Fabrication of large area ultrathin silicon membrane: Application for high
> efficiency extreme ultraviolet diffraction gratings*
> C. Constancias,a B. Dalzotto, and P. Michallon
> CEA Grenoble-MINATEC, 17 rue des Martyrs, F38054 Grenoble, France
> J. Wallace
> Center for NanoTechnology, University of Wisconsin-Madison, 425 Henry
> Mall,
> Suite 2130,
> Wisconsin 53706
> M. Saib
> CNRS-LTM Grenoble-MINATEC, 17 rue des Martyrs, F38054 Grenoble, France
> Received 20 July 2009; accepted 14 December 2009; published 28 January
> 2010
> Silicon membranes of 100 nm thick and below over several mm2 have been
> fabricated for high
> efficiency extreme ultraviolet EUV transmission grating. The perfect
> planarity 1 nm and the
> high transparency 80% at 13.5 nm wavelength have been measured. In
> comparison to SiNx
> membranes 40% transmission, the silicon membranes allow high resolution
> EUV interference
> lithography using the second order diffraction of the molybdenum grating.
> The fabrication of such
> phase gratings has been performed and the diffraction efficiency
> measurement
> is 27% for the silicon
> membrane and the Mo grating. C 2010 American Vacuum Society. DOI:
> 10.1116/1.3290746
>
> Marco
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review