A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Electroplated FeNi Analysis. Calibration Standard
Electroplated FeNi Analysis. Calibration Standard
2011-11-09
Denis Petrov
2011-11-18
David Roberts
Electroplated FeNi Analysis. Calibration Standard
Denis Petrov
2011-11-09
Dear colleagues,

we are about to electroplate 20Fe80Ni layer onto our wafers. We have to
fullfill a very strict spec concearning the percentage of Fe in this layer.
Among other methods, we are going to use an EDX-analyser. But we lack a
calibration standard for 20Fe80Ni alloy.

Could anyone suggest a good and reliable supplier of such standards
(preferrably in Europe, since we will need it very soon)?

Many thanks in advance!

Best regards,

--
Denis Petrov
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.