What's the shear strength of silicon?
2012-06-21
Yingnan Wang
2012-06-27
Tang Tian
What's the shear strength of silicon?
Yingnan Wang
2012-06-21
Dear all,Could anyone advise the shear strength of silicon? Any orentation would
be ok.I've been searching for the data in vain.Thanks in advance for any
help.All the best,WANG, Yingnan
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Addison Engineering
MEMS Technology Review