MEMSnet Home: MEMS-Talk: Removal of crosslinked SU8
Removal of crosslinked SU8
2012-07-17
Yingtao Tian
2012-07-17
Karim Ogando
2012-07-17
Yingtao Tian
2012-07-17
Mike Whitson
2012-07-17
Shay
2012-07-17
Ad Hall
2012-07-17
Lukasz Urbanski
2012-07-20
Matthieu Nannini, Dr.
Removal of crosslinked SU8
Karim Ogando
2012-07-17
Hi Yingtao,

Maybe you can use O2 Plasma, but it is going to damage the thin oxide
film on the top of the chrome.

which is the thickness of the crosslinked SU8?

Best regards,

Karim

On Tue, Jul 17, 2012 at 11:16 AM, Yingtao Tian  wrote:
> Hi All,
>
> I have a chrome/glass mask seriously contaminated by crosslinked SU8, anyone
has an idea how to rescue the mask?
>
> Thanks,
> Yingtao
>
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer