Dicing silicon with diamond blade
Emre Olceroglu
2013-01-30
Hello,

I was wondering if I can dice 0.5mm silicon wafers with diamond blades
that we normally use for Pyrex dicing.

I know people dice bonded Silicon-Pyrex but I am not sure which blade
they use.

Thanks.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics