A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SU8 for Au Plating
SU8 for Au Plating
2013-03-19
Jocelyn Ng
2013-04-04
Kevin Nichols
2013-04-04
Michael Martin
2013-04-03
André Bödecker
2013-04-03
Bill Moffat
2013-04-04
Jocelyn Ng
2013-04-04
André Bödecker
SU8 for Au Plating
Bill Moffat
2013-04-03
Joycelyn,
                  Missed your email.  Get in contact with me and I will send you
details of sub-micron metal pillars, 10 micron metal pillars and up to 30 micron
metal pillars using either standard positive resist or photosensitive polyimide.
Bill Moffat

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of André
Bödecker
Sent: Wednesday, April 03, 2013 1:52 AM
To: [email protected]
Subject: [mems-talk] SU8 for Au Plating

Dear Jocelyn,



what is the reason for you to use SU-8? This resist is designated as a permanent
resist so it is quite unsuitable for plating processes in the case you want to
remove it afterwards. For such applications I would recommend a normal positive
resist.



Best regards,

André Bödecker



_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search