MEMSnet Home: MEMS-Talk: microcantilever fabrication
microcantilever fabrication
2013-10-23
girija moona
2013-10-23
Salem Saadon
2013-10-24
MRC gmail
2013-10-24
Denis Petrov
2013-10-28
Chayanika Josh
2013-10-23
Wolinski, Jeffrey P
2013-10-24
alaa melhem
microcantilever fabrication
Denis Petrov
2013-10-24
Hi Girija,

in fact, there are numbers of ways of how to fabricate a microcantilever
beam.
A lot of them are described in books on MEMS technology (i.e. Menz, Mohr,
Paul). But it is difficult to answer your question since you do not even
describe, which procedure you are going to use (bulk or surface
micromachining) and which material should the cantilever be fabricated
from. For example, a cantilever can be metallic, bimetallic, or polysilicon.

In either way you will most probably have to  fabricate a microstructure
(cantilever geometry) using microlithography and then underetch the
sacrificial matereal to make the beam moveable.


Regards,
Denis



2013/10/23 girija moona 

> hello everyone,
> it would be great if someone could help me microcantilever fabrication. i
> need all the steps in detail... since in am very new to this field and want
> to work in the area to microcantilever sensors. i will be very thankful if
> i get some basic procedure for microcantilever fabrication.
> thanks
>
> Regards
> Girija Moona
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>



--
--
День

The Band "Don't Pushkin"

http://vkontakte.ru/club7171559

http://www.dontpushkin.com 
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group
Tanner EDA by Mentor Graphics