MEMSnet Home: MEMS-Talk: Best recipe to etch sio2 using CHF3 gas with ULVAC NE-550
Best recipe to etch sio2 using CHF3 gas with ULVAC NE-550
2014-05-19
Ryan
2014-05-19
Martin,Michael David
2014-05-20
Ryan
2014-05-21
Martin,Michael David
Best recipe to etch sio2 using CHF3 gas with ULVAC NE-550
Ryan
2014-05-20
Thanks Michael.



Otherwise, if source power is lower than bias, does it damage wafer or
interrupt uniformity and etch rate?

In addition, back side cooling (He) ??



Regards,



Ryan



EXCELSIOR

Manager

Ryan Hyunmin Kim

E : [email protected]

M: +82-10-3802-2229



_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation