Hi Abdul,
My specialty is wafer electroplating, but either way one must make
electrical contact to the wafer. I can help you with electro-process
tooling if you can describe the chemicals you will be using. Also include
some company/organization information.

Thank you,
Dave

David Roberts (Principal)
Silicon Valley Wafer Plating
807 Aldo Ave. Ste. 107 Santa Clara, CA 95054
(408) 469-3203
www.waferplating.com

> Hello
>
> I want to develop Electrochemical Etch Stop process. For this purpose I'll
> use Epi wafer (Substrate = P-type Si, [100], 500um thick, and Epi-layer =
> N-type, 10um thick). I have also MEMS Potentiostat from "AMMT". I'll be
> thankful if someone can provide information on it.
>
> Thanks
> --
> Abdul Qader Ahsan
>
>


Best regards,
Dave

David Roberts (Principal)
Silicon Valley Wafer Plating
807 Aldo Ave. Ste. 107 Santa Clara, CA 95054
(408) 469-3203
www.waferplating.com

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group