Hello:

We are looking for a source of selective tungsten deposition for out 5-inch
wafers and individual die. We wish to selectively deposit tungsten on
aluminum pads, but not on silicon nitride. If you are interested in helping
us perform this process, please contact me as listed below.

Milam Pender
Trex Enterprises
590 Lipoa Parkway, Suite 222
Kihei, HI 96753
(808) 875-2640 (Office)
(808) 875-2611 (Fax)
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing