Dear Dr. Walsh,

We use Dupont Photomasks to make our masks and they seem to have the highest
quality and the highest prices. They may however, be good to work with.  Our
service representative is Leonard Perry, (512) 310-6105.  Another company we
have used and our happy with is Align-Rite, Craig Durgy, 203 577-4020.  They
are a bit less expensive.

Allen Cowen
(919) 248-1424
[email protected]

Kevin M Walsh wrote:
Could people give me recommendations for a vendor who will produce patterned

> 5" chrome photomasks for universities at a decent price to be used in a
> 1:1 contact aligner. I have several masks to be made.
>
> Thanks,
> Kevin Walsh
>
> --
> Dr. Kevin M. Walsh
> Electrical Engineering Department, Speed Scientific School
> University of Louisville, Louisville, KY 40292
> (502) 852-0826
>
> Internet address: [email protected]
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Mentor Graphics Corporation