Dear members

I am looking for a glue with the following specifications
1) medium viscosity before hardening, 2000cps
2)1 component glue
3)no UV-curing, and no heating process for hardening
4)low shrinkage during hardening (<3%)
5)low exo- and indo thermic process during hardening
6)good adhesion to glass and stainless steel  from 0 to 80C, for at least
10 years
7)low CTE : <50*10^-6 K^-1 after hardening
8)complete hardening time below 20min.
9)Operationtemperature: 0- >100C
10)>24,5 N/mm^2 in shear strength from 0-80C

I have been trying several glues without success. No glue could match all
these specs at the same time. So if you have tried to use  a glue as above
described please let me know, I am still not satisfied with all the glues
the vendors have sold me.

Mounir Ennabli, R&D Engineer

=======================================================
Mounir Ennabli || IBSEN Micro Structures A/S
Gammelgaardsvej 65 | DK-3520 Farum | Denmark
Tel.: (+45) 44 99 55 60 | Fax.: (+45) 44 99 55 61
[email protected] | http://www.ibsen.dk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer