A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Boron diffusion problem
Re: Boron diffusion problem
1995-11-25
robert s okojie ee stnt
1995-11-29
Padmaja Ramadas
Re: Boron diffusion problem
robert s okojie ee stnt
1995-11-25
Zheng,

I suspect you may be experiencing surface induced damage due to direct
diffusion into silicon.

If your process flow permits, try growing a layer of oxide(say 3000angs, wet)
before diffusing. Strip the oxide after that.

Deep diffusion is generally problematic, hence the above solution may not be a
perfect one.

Goodluck.

Robert S. Okojie
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics