There are a few possibilities:
1. DSC (= Dynamic Scanning Calorimetry?)
2. TMA (= Thermo Mechanical Analysis)
Equipment is available from Perkin Elmer, Mettler and others.

Greetings

Armin Kuebelbeck

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing