Dear all,

As far as I know, the only use of permanent magnets in MEMS are the ones we use
in our thin film magnetic heads. We are depositing and structuring those magnets
for over six years in production in our Magnetic head/MEMS foundry.

Henne van Heeren
OnStream BV
Eindhoven, The Netherlands
tel 31 40 27 24246
fax 31 40 27 22259
email [email protected]

The main use of permanent

----------
From:   Giovanni Zangari[SMTP:[email protected]]
Reply To:       [email protected]
Sent:   Thursday, February 18, 1999 1:25 AM
To:     [email protected]
Subject:        Permanent magnets in MEMS

0100,0100,0100Hi all:


the recent enquiry by 0000,0000,8000Suresh G.K.
Ananthasuresh

on permanent magnet membranes triggers another question, that I
hope many of you will have answers to:

what are the main uses of permanent magnets in MEMS?

what are the applications where the availability of permanent
magnet films would be important?

are there current applications or papers where a permanent magnet
film is used?


Thank you in advance for all your help.


     Giovanni



===================================================
Dr. Giovanni ZANGARI
Assistant Professor
Dept. of Metallurgical and Materials Engineering
University of Alabama
P.O. Box 870202, 120 Bevill Building
Tuscaloosa, AL
Phone:  (205) 348-7074
Fax:    (205) 348-2164
e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing