1999-02-02
CNF can do it.

How thick.
What doping level
What kind of substrate.

How many.


Lynn


>This is a multi-part message in MIME format.
>--------------2A219C626459F18EFAE28638
>Content-Type: text/plain; charset=us-ascii
>Content-Transfer-Encoding: 7bit
>
>Does anybody know a source for CVD of in-situ boron doped polysilicon?
>I want to do this on 3" squre substrate.
>
>Please let me know.
>
>Thanks
>
>Matt
>
>--------------2A219C626459F18EFAE28638
>Content-Type: text/x-vcard; charset=us-ascii; name="vcard.vcf"
>Content-Transfer-Encoding: 7bit
>Content-Description: Card for Matthew Wilcox
>Content-Disposition: attachment; filename="vcard.vcf"
>
>begin:          vcard
>fn:             Matthew Wilcox
>n:              Wilcox;Matthew
>org:            MEMS Inc.
>adr;dom:        MEMS Inc.;;5650 Stewart Avenue;Fremont;CA;94538;
>email;internet: [email protected]
>tel;work:       (510)657-7616
>tel;fax:        (510)657-8906
>tel;home:       Home Office (510)770-1246
>x-mozilla-cpt:  ;0
>x-mozilla-html: FALSE
>version:        2.1
>end:            vcard
>
>
>--------------2A219C626459F18EFAE28638--
>
>


*****************************************************
Dr. Lynn Rathbun, User Program Manager   Voice (607)-255-2329 ext 110
Cornell Nanofabrication Facility                    FAX(607)-255-8601
Knight Laboratory-Cornell University    email   [email protected]
Ithaca, New York 14853                      http://www.cnf.cornell.edu/
Webmaster @ Christian World Adoption  http://www.cwa.org/
Webmaster @ Joint Council on International Children's Services www.jcics.org
(any opinions or representations of fact re: adoption are my own however)
*****************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing