We are interested in shock testing data on both surface michomachined devices
and bulk silicon mems, such as actuators, mirrors, shutters, etc. There are two
ranges of interest, low, brief shocks (mishandling, dropping from 5 to 40 feet,
etc.- after packaging that is) and their survivability in the range of kG's. If
you have any information you wish to share or know of a potential source,
please respond to the [email protected] address rather than my own so that any other
interested parties may also share in it. Thank you!

shirley
-------------------------------------
Shirley Kidner
E-mail: [email protected]
06/05/95
13:30:35
-------------------------------------


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Addison Engineering
Tanner EDA by Mentor Graphics