MEMSnet Home: MEMS-Talk: Re: selective etching of Cu (Ag) over alumina
Re: selective etching of Cu (Ag) over alumina
1999-05-05
Zhen YANG
1999-05-05
[email protected]
1999-05-05
[email protected]
Re: selective etching of Cu (Ag) over alumina
[email protected]
1999-05-05
Dear Dr. Zangari,

Ferric chloride, FeCl2 will etch copper. I believe it will leave the aluminum
alone, especially with the oxide layer present. You can pick it up at the
local Radio Shack store. It is used for etching PC boards.

Good luck,
Michael Mattes
 MicroMechatronics


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer
MEMStaff Inc.