I am wondering if there is a recipe (assuming it's possible) for
bonding together two wafers, one with a Silicon surface, and the
other with a polyimide coating? Can it be done with just heat and
pressure?


Thanks,
John Neumann
--

%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%

Dr. John Neumann
Postdoctoral Researcher, ECE Dept.
Micro-electro-mechanical Systems (MEMS)
1209 Hamerschlag Hall
Carnegie Mellon University
Pittsburgh, PA 15213-3890

[email protected]
phone: (412) 268-4404
FAX: (412) 268-2860


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMStaff Inc.