I am very interested in the techniques that lead to formation of
nano-porous Au films or what is sometimes referred to as "gold black"
(in fact, nano-porous gold is not necessarily black).

As I could identify from literature, there are the following approaches
to nano-porous gold:

1. Electrochemical etching
2. Assembling gold colloidal particles (particularly, using polystyrene
nano-beads as template)
3. Thermal evaporation in the inert atmosphere under high pressure
4. Laser ablation
....
Is there anything else that can be used to prepare nano-porous Au films?

Your information will be highly appreciated.


(In return, I would be happy to provide the references for the
techniques I have mentioned)

--
Nickolay Lavrik
University of Tennessee
Department of Chemistry
420 Buehler Hall

Ph.(865) 974-6174


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering