MEMSnet Home: MEMS-Talk: Re: Looking for glass (7740) substrate supplier
Re: Looking for glass (7740) substrate supplier
1996-04-03
Jeffrey M. Melzak
1996-04-04
Ash Parameswaran
Re: Looking for glass (7740) substrate supplier
Jeffrey M. Melzak
1996-04-03
We have purchased such substrates (4") from Esco Products in the past. They are
at 171 Oak Ridge Rd., Oak Ridge, NJ 07438-0155. Phone is (201)697-3700, fax is
(201)697-3011. Price (as of 2 years ago) was $45.00 for 4" 20-mil pyrex 7740
wafers with 60/40 finish.

Jeff Melzak
CWRU


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation