Dear colleagues,

I am searching for a coating to protect silicon and alu connection strips from
water. The device we are making, gets immersed in the water.
We already used parylene as a coating, but this has bad wetting properties, so
we are searching for an alternative.
Any suggestions are welcome.
Thanks in advance,

Martin De Kegelaer
email: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
University Wafer