2000-12-27
[email protected]
A question about Ni
[email protected]
2000-12-27
dear professor:
    I am a postgraduate student from Tsinghua Univ of China.
    I have a question to ask. Has a sputtered Ni layer a compressive residual
stress? Then what is the usual value?
Thank you for your help.
                                           yours truly
                                            Suyan Liu
                                            2000.12.4



_____________________________________________
Ê×¶¼ÔÚÏß--ÖйúÈ˵ÄÍøÉϼÒÔ° http://www.263.net
@263.netÖйú×î´óµÄÔÚÏßÓÊ¾Ö http://freemail.263.net
ÖйúÈ˵ÄÔÚÏß¹ºÎïÀÖÔ°¡ª¡ª263ÉÌ³Ç http://shopping.263.net
ÍøÉÏÁôѧ×Éѯ-Öйú½ÌÓý·þÎñÍø http://edu.263.net/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing