Protecting Coating for KOH etch
2001-03-16
Asif Aziz
Protecting Coating for KOH etch
Asif Aziz
2001-03-16
Please can anyone suggest a suitable coating to protect Si surface from
etching in KOH.


[email protected]

Asif Aziz
Department of Physics and Astronomy
Kelvin Building
University of Glasgow
University Avenue
Glasgow
G12 8QQ

Tel. no. +44 141 339 8855 extn 0896