We are looking for a service that can do thick plating and selective etching
of silver on six-inch wafers. We need to create silver bumps approximately
75mm in height by 150mm in diameter. Please send me any information on
companies that might be able to offer this service.

Thanks,
Peter Wright
Triquint Semiconductor