Kenneth Smith
Re: FZ High Resistivity 150 mm Silicon Wanted
Kenneth Smith
2001-06-07
John,

If you have not found these wafers yet, I can offer you some N type 150
mm at > 4000 ohm-cm. I know that this quite below your request, but if
you can use this range, please contact me.

Regards,

Ken Smith

"Koons, John" wrote:
>
> Readers,
>
>   I'm looking for several pieces (<10) of high resistivity silicon which
> needs to be 150 mm diameter and on the order of 10,000 ohm-cm.
> I have resource listings on where to get silicon manufactured to meet
> this - I'm just trying to purchase a few loose pieces to steer clear of
> the minimum quantity numbers for now. If anyone knows of a small
> supply that's gathering cleanroom dust somewhere, I'll put it to
> good use. Thanks in advance.
>
> John
>
>
> John M. Koons
> Process Engineer
> Innovative Micro Technology
> 805-681-2816
> [email protected]

--
Ken Smith

Kmbh Associates

4968 Charter Road
Rocklin, CA  95765  USA
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
University Wafer