Dear Vittorio,

We are very satisfied with Degussa: http://www.degussa.com/index_en.cfm

best regards

Henne van Heeren
OnStream MST B.V.
Lodewijkstraat 1
5652 AC Eindhoven
The Netherlands
tel +31 40 295 9815
mobile: +31 622 60 3120
fax +31 40 295 9906
[email protected]

The Micromachining foundry

OnStream MST Confidential

-----Original Message-----
From: Vlttorio Guarnieri [mailto:[email protected]]
Sent: Friday, September 28, 2001 9:52 AM
To: [email protected]
Subject: [mems-talk] gold electroplating bath


I am working on electroplating bath for gold deposition (electronic grade);
now we use cianide bath but it eats the photoresist mask! I am looking for
companies providing these kind of products, in particular I am interested in
ammonium sulfite gold bath but in general I need informations about
companies working in this field.

regards
Vittorio Guarnieri

Dott. Ing. Guarnieri Vittorio
MicroSystemDivision ITC-Irst
Via Sommarive, 18
38050, Povo, Trento
Italy
tel: +39 0461 314468
fax:  +39 0461 314591
[email protected]
_______________________________________________
mems-talk mailing list
[email protected]
To unsubscribe or change your list options, use:
 http://fab.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing