Surface Roughness
2001-11-09
Jiangang Du (John Duke)
2001-11-11
martin.walker4
Surface Roughness
martin.walker4
2001-11-11
Try AFM (Atomic Force Microscopy).  This is one of the few techniques that
can operate at this level.  If your sample is conductive, you can use the
variant known as Scanning Tunneling Microscopy, which allows a few other
things to be learnt about the sample.  The biggest supplier of AFMs is
probably Digital Instruments.  Check their website for more information on
the technique.

Regards,

Martin Walker (Oxford Instruments)
----- Original Message -----
From: "Jiangang Du (John Duke)" 
To: 
Sent: Saturday, November 10, 2001 3:27 AM
Subject: [mems-talk] Surface Roughness


> Dear all,
> Can anybody recommend my a method or a instrument that will measure
surface roughness down to 1 anstrom.
> Thanks a lot
>
>
>
>
>
> Regards,
>
> John Duke
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review