MEMSnet Home: MEMS-Talk: Re: mems-talk digest, Vol 1 #103,developing photoresist
Re: mems-talk digest, Vol 1 #103,developing photoresist
2001-11-26
Marty Patton
Re: mems-talk digest, Vol 1 #103,developing photoresist
Marty Patton
2001-11-26
Negative photoresist does that under certain conditions.  Try Futurrex
negative resist used in liftoff processing.