Question for SU-8 photoresist adhesion problem.
2001-12-05
Tao Xu
2001-12-05
BERAUER,FRANK (HP-Singapore,ex7)
Question for SU-8 photoresist adhesion problem.
BERAUER,FRANK (HP-Singapore,ex7)
2001-12-05
SU-8 cannot withstand KOH. It is chemically attacked
by KOH and I am afraid nothing can change that.
You may use TMAH instead, which does not attack SU-8.
But even then adhesion is a challenge.
Please contact me if you need more information.

Greetings,
        Frank Berauer
        Senior R&D Engineer
        Hewlett-Packard Singapore


-----Original Message-----
From: Tao Xu [mailto:[email protected]]
Sent: 5 December 2001 14:50
To: [email protected]
Subject: [mems-talk] Question for SU-8 photoresist adhesion problem.


Hi,

    I met a question about SU-8 photoresist adhesion.
    I spun SU-8 on the SiO2/Si or Si3N4/Si substrate. After pattern the
SU-8, I put them into 30% KOH solution (80 degree C) to etch Si to form the
V-groove. However, SU-8 peeled off very quickly (just 1-2min) in the KOH
solution. The SU-8 is a part of my device and I want it to stay there after
KOH etching.
    Did anybody meet this problem and know how to solve it? Any suggestion
is high appreciation. Thanks in advance.

Regards,

Tao

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering