MEMSnet Home: MEMS-Talk: effect of ammonium flouride
effect of ammonium flouride
2001-12-18
Ken Kwon
2001-12-19
Luiz Marangoni
2001-12-20
Ravi Shankar
effect of ammonium flouride
Luiz Marangoni
2001-12-19
Hi Ken,

I4m starting to work with porous silicon and I found some reference about
ammonium fluoride as electrolyte in the process of PS formation. The main
advantage of the ammonium fluoride, in this case, is that it etches the
alumminum with a rate of about five times lower than HF etches. If do you
want I can pass the reference to you (or the pdf file).

Bye,
Luiz Marangoni
[email protected]




>Hello,
>
>     I am looking for a literature or an article about effect of using
> ammonium flouride in oxide wet etching (BOE) and in isotropic silicon wet
> etching.  I know that it is acting as a buffer but I want to know about
> its mechanism and any experiment results showing why ammonium flouride is
> prefered in some cases.
>
>Thank you.
>
>Ken.
>
>
>_________________________________________________________________
>Send and receive Hotmail on your mobile device: http://mobile.msn.com
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/
>
>
>
>
>
>---
>Incoming mail is certified Virus Free.
>Checked by AVG anti-virus system (http://www.grisoft.com).
>Version: 6.0.307 / Virus Database: 168 - Release Date: 11/12/01

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation
The Branford Group