adhesion of TaN to quartz
2002-01-16
adnan merhaba
2002-01-16
[email protected]
adhesion of TaN to quartz
[email protected]
2002-01-16
Try an oxygen plasma or a clean step with argon in your sputtering system
prior to deposition. Bob Henderson