Haze on HF:Nitric etched silicon
2002-01-23
[email protected]
2002-01-23
Maurice Norcott
Haze on HF:Nitric etched silicon
[email protected]
2002-01-23
I am interested in cause of sporadic cloudiness which could be 'haze' on
silicon surfaces etched using dilute HF:Nitric, any insight or useful
references would be gratefully received.

Thanks in advance,

Sarah Sharp
Senior Technologist
Oxford Instruments Analytical



 ###  OXFORD INSTRUMENTS   http://www.oxford-instruments.com/  ###

Unless stated above to be non-confidential, this E-mail and any
attachments are private and confidential and are for the addressee
only and may not be used, copied or disclosed save to the addressee.
If you have received this E-mail in error please notify us upon receipt
and delete it from your records. Internet communications are not secure
and Oxford Instruments is not responsible for their abuse by third
parties nor for any alteration or corruption in transmission.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.