A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: wet etching of Au
wet etching of Au
2002-02-11
Oberhammer Joachim
2002-02-11
Roger Shile
wet etching of Au
Roger Shile
2002-02-11
I  use Transene TFA Gold etchant, which is a solution of iodine and potassium
iodide.  I don't believe it will significantly attack any of the other
materials you mentioned.

Roger Shile

>>> [email protected] 02/11/02 01:31AM >>>
I have to etch Au layers of different thicknesses ranging from 100 nm to 2
um.

I found different chemicals to etch gold: (1) KI:I2:DI H20=4:1:40
(weight), (2) HCL:HNO3:DI=4:4:9 (volume), (3) HCL:HNO3:DI H20=3:1:?
("king's water")

Does anybody know about the selectivitiies of such etchants to Al
(!!), SiO2, SiN, Cr, Si. Do you have experiences with these etchants
regarding uniformity, etching rates, selectivity, suitable mask
materials? Which one could you recommend?

Thanks a lot for your answer(s).
--
-----------------------------------------------------------------------------
-
Joachim Oberhammer, Dipl.-Ing.

Royal Institute of Technology (KTH)   Phone:    +46/(0)8 790 6250
Dep. of Signals, Sensors and Systems  Fax:      +46/(0)8 10 0858
Microsystem Technology (MST)          Mobile:   +46/(0)70 692 1858
                                       e-mail:   [email protected]
Osquldas vdg 10                       homepage: http://www.s3.kth.se/mst/
SE-100 44 Stockholm, Sweden
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation