MEMSnet Home: MEMS-Talk: BCB Removal from Silicon
BCB Removal from Silicon
2002-02-08
Renie M Duvall
2002-02-15
Greg Miller
BCB Removal from Silicon
Greg Miller
2002-02-15
Renie,

A plasma etch CF4 O2 will do the trix -
I been told Xylene works but it seems to take a long time
Also, Hot Sulfric and Peroxide 75 to 25 will do the trix in a short
amount
Greg Miller
KVH Industries

-----Original Message-----
From: Renie M Duvall [mailto:[email protected]]
Sent: Friday, February 08, 2002 11:32 PM
To: [email protected]
Subject: [mems-talk] BCB Removal from Silicon


Is there anyone that knows a method or vendor that can remove BCB from
silicon, "cyclotene" produced by Dow?  I understand that  the solvent
mesitylene will work but do not know any vendor source or other method
for removal.  --- Renie M Duvall--- [email protected]
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing