kumar m.v.n buduri
Teflon coated pyrex glass wafer bonding
kumar m.v.n buduri
2002-03-05
Hai

I would like to know how two pyrex glass wafers spin
coated with teflon AF 1600/2400 can be bonded.(both bonded sides
 are coated with teflon).Please provide me with details of recepie/procedure.
thank you