MEMSnet Home: MEMS-Talk: Re: Etchant for Cr
Re: Etchant for Cr
1996-07-17
Alexander Barr
1996-07-17
Johan Drott
1996-07-18
Mac McReynolds
1996-07-19
Christopher G. Levey
Re: Etchant for Cr
Christopher G. Levey
1996-07-19
We use CR7S chromium etchant from Cyantek Corp.
[(510) 651-3341] for etching chrome masks.  It is
effective and inexpensive (~$25/gal).

--- Behrouz Nikpour WROTE:
> Hello,
>
>  I need to pattern Cr which is deposited on Glass. Does anybody know an
etchant
> for Cr that does not attack photoresist?
>
> thanks
> Behrouz Nikpour
> Dept. Elec. Eng.
> Concordia University


--
--Chris Levey
  Director, Microengineering Lab
  Thayer School, Dartmouth College
  email: [email protected]
  http://hypatia.dartmouth.edu/levey.html


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics