Dear MEMS society,

I want to make holes (diameter 3-5 um, depth 40-50 um) in a QUARTZ substrate
by DRIE etching.
Which mask materials, photoresist,... should be used?
Any comments and/or etch recipes are welcome.

Thanks

Regards