MEMSnet Home: MEMS-Talk: Re: Thermal expansion coefficient of oxide film
Re: Thermal expansion coefficient of oxide film
2002-03-11
Craig McGray
Re: Thermal expansion coefficient of oxide film
Craig McGray
2002-03-11
Hello Jia Zhou,

One of many places to find the thermal expansion coefficient of silicon dioxide
is as follows:

Milton Ohring
"The Materials Science of Thin Films"
Academic Press, San Diego California
1992

The value provided in this text is 0.55 ppm/K.

Please keep in mind that this value will vary depending on how the oxide was
produced.

Best Wishes,
Craig McGray
Dartmouth College


[email protected] wrote:

> Message: 9
> From: Jia Zhou 
> To: [email protected]
> Date: Mon, 11 Mar 2002 07:44:36 -0600 (CST)
> Subject: [mems-talk] Thermal expansion coefficient of oxide film
> Reply-To: [email protected]
>
> Wher can I find the thermal expansion coefficient of silicon oxide film.
Thanks.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation