MEMSnet Home: MEMS-Talk: Problem in etching Al and Pt
Problem in etching Al and Pt
2002-03-04
Hoyin
2002-03-06
Greg Miller
2002-03-08
Yun-Ju Chuang
2002-03-13
Chan Ho Yin
Problem in etching Al and Pt
Chan Ho Yin
2002-03-13
Hi,

        If I use AZ400K to etch Al, what is the mask I should use? I try
to use AZ5214 PR. But not very good...Some of the pattern is etched.

Thank you

Hoyin

On Fri, 8 Mar 2002, Yun-Ju Chuang wrote:

> Hi,
>
> Besides AZ MIF327, you may try AZ 400K developer.
> I think you could try this Al etchant  H3PO4:HNO3:CH3COOH:DI=16:1:1:2 .
> We used this etchant to pattern Al as interconnecton line on Pt resistor.
>
> Yun-Ju Chuang
>
> ----- Original Message -----
> From: "Greg Miller" 
> To: 
> Sent: Thursday, March 07, 2002 6:23 AM
> Subject: RE: [mems-talk] Problem in etching Al and Pt
>
>
> > You might want to try AZ MIF 327 Photoresist developer - you might stand
> > a better chance of etching your Al film - its very slow but works quite
> > well.
> >
> > Greg Miller
> > KVH
> >
> > -----Original Message-----
> > From: Hoyin [mailto:[email protected]]
> > Sent: Monday, March 04, 2002 9:38 AM
> > To: [email protected]
> > Subject: [mems-talk] Problem in etching Al and Pt
> >
> >
> >  Hi all,
> >
> >      I have got a simple question.   I want to sacrifically release my =
> >  device by etching Al. However, one of the layer is Pt. Will the Al =
> >  etchant etch Pt  ???  What etchant do you suggest??
> >
> >  Thank you very much!!!
> >
> >  Hoyin
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.mems-exchange.org/
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.mems-exchange.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering